ASTM-D3150:2006 Edition
$35.75
D3150-00(2006) Standard Specification for Crosslinked and Noncrosslinked Poly(Vinyl Chloride) Heat-Shrinkable Tubing for Electrical Insulation
Published By | Publication Date | Number of Pages |
ASTM | 2006 | 3 |
1.1 This specification applies to flexible, crosslinked and noncrosslinked poly(vinyl chloride) heat-shrinkable tubing for electrical insulating purposes. It is supplied in an expanded form and will shrink to its extruded diameter when heated.
Note 1This standard is similar but not identical to IEC 60684-3-201.
1.2 The values stated in inch-pound units are to be regarded as the standard except temperature, which shall be stated in degrees Celsius. Values in parentheses are for information only.
PDF Catalog
PDF Pages | PDF Title |
---|---|
1 | Scope Referenced Documents Terminology Classification Ordering Information Materials and Manufacture Chemical and Physical Property Requirements |
2 | Dimensional Requirements Workmanship Sampling TABLE 1 TABLE 2 |
3 | Number of Tests and Retests Test Methods Inspection Certification Packaging, Marking, and Shipping Keywords TABLE 3 TABLE 4 |